MUMBAI, India, Nov. 13 -- Intellectual Property India has published a patent application (202511039346 A) filed by Indian Institute Of Technology Delhi on April 24, 2025, for Hybrid Flame Post-Treatment Process Of High Velocity Air Fuel Sprayed Nickel Based Superalloy Coatings.
Inventors include Bhowmik, Ayan; Raj, Sanjay; Kumar, Deepak; Kumari, Sudha; N V, Abhijith; Mondal, Chandan; and Gosvami, Nitya Nand.
The application for the patent was published on November 13, 2026, under issue no. 46/2026.
Abstract: The present invention discloses a novel high velocity oxy-acetylene flame treatment as a low-cost technique on Ni-based superalloy (Inconel 718) coatings produced by high-velocity air fuel (HVAF) methods. The process is very suitable for imparting superior microstructural and mechanical properties of the super alloy coatings compared to the conventional HVAF sprayed coatings. The FT-HVAF process is capable of addressing the shortcomings (porosity and poor interlamellar bonding) of HVAF coatings. The result shows a 30–50% reduction in porosity and a transformation of dendritic structures into finer, more uniform grains.
Disclaimer: Curated by HT Syndication.