MUMBAI, India, Nov. 6 -- Intellectual Property India has published a patent application (202641130646 A) filed by M. Kumarasamy College Of Engineering; K. Ramakrishnan College Of Engineering; and K. Ramakrishnan College Of Technology on November 02, 2026, for Development Of Eco-Friendly Paver Block Using Bakelite And Seashell.
Inventors include Srinivasan Palanisamy; Mukesh Panneerselvam; Suvetha Ganesamoorthi; Harish Ragupathi; Pranav Maran Thirumaran; Rahulkandhasamy; Balakumar A; and Oviya R.
The application for the patent was published on November 06, 2026, under issue no. 45/2026.
Abstract: ABSTRACT DEVELOPMENT OF ECO-FRIENDLY PAVER BLOCK USING BAKELITE AND SEASHELL In the present age, waste management has become a critical global challenge faced by various regions in the world. Here, Plastic is significantly growing segment in the municipal solid waste. So, Our Project aims to develop eco-friendly paver blocks using seashell, which was available abundantly and waste material Bakelite as a partial replacement for natural aggregates. The Ordinary Portland Cement (OPC 43) was used as the primary binding material. The Seashells are collected from the coastal regions, cleaned and then crushed into fine aggregate size. The seashell was mixed in the 1:1 ratio of mussel shell and snail shell. The seashell was added in the ratio of 70:30 and 75:25, here the 70% is seashell and 30% is seashell. Bakelite waste is used as the partial replacement for coarse aggregate. And the Bakelite are collected from the plastic recycling shop and then crushed into the particle size of coarse aggregate. The Bakelite was added to the coarse aggregate into 4% and 6%. And then the prepared mix was moulded into the standard paver block sizes and allowed for curing for 28 days. The test for the paver block was conducted as per IS 15658:2006. As the result, the ratio of 70:30 of M- sand and seashell with 4% of Bakelite achieved the compressive strength of 42 MPa, water absorption of paver block was 3% and flexural strength of 5 MPa. And the ratio of 75:25 of M-sand and seashell with 6% of Bakelite showed the compressive strength of 48MPa, water absorption of 2.6% and the flexural strength of 6.5MPa. In both cases, the performance value meets the standard value as per BIS requirements.
Disclaimer: Curated by HT Syndication.