MUMBAI, India, Nov. 6 -- Intellectual Property India has published a patent application (202511035641 A) filed by Chairman, Defence Research & Development Organization Drdo; and Principal, Sri Ramakrishna Engineering College Srec on April 11, 2025, for A Method To Alleviate Blackening In Anodized Additive Manufactured Alsi10mg Alloy Through Heat Treatment..
Inventors include Chandramohan Palanisamy; Raghu Raman; Chandan Mondal; Pradeesh Kumar Dhanaraj; and Saravanakumar Shanmugam.
The application for the patent was published on November 06, 2026, under issue no. 45/2026.
Abstract: A method to alleviate blackening in anodized Additive Manufactured AlSi10Mg alloy through heat treatment. This invention presents a method for alleviating blackening in anodized Additive Manufactured (AM) AlSi10Mg alloy through heat treatment processes. The method involves creating AlSi10Mg alloy samples using Direct Metal Laser Sintering with specific parameters, followed by two different heat treatment approaches: Solution Heat Treatment (SHT) at 430°C to 500°C for 0 to 2 hours, followed by artificial aging at room temperature from 0°C to 140°C for 0-9 hours with water cooling. Stress Relieving (SR) at 250°C to 290°C for 0-2 hours, followed by air cooling at room temperature. After heat treatment, the samples undergo a multi-step anodizing process involving caustic soda treatment, washing, nitric acid treatment, and anodizing at specific voltages. Visual inspection reveals that SHT samples appear darker (black), while SR samples appear lighter (grey). The mean intensity of the blackening is measured with Python 3.10 software with an 8-bit grayscale system. It is observed that SHT samples having a high intensity of 36.69 to 44.12 and SR samples having a low intensity of 44.46 to 63.58 of blackening. Microstructure analysis using FESEM characterization shows that SHT samples have a coarser silicon distribution, while SR samples have a finer silicon distribution. The finer silicon distribution and low intensity of blackening were achieved through the SR heat treatment process is found to alleviate the formation of blackening in anodized AM AlSi10Mg alloy. This method addresses the challenge of blackening in anodized AM AlSi10Mg alloy, which is crucial for enhancing the corrosion resistance and effectiveness of components used in the aerospace and defense sector.
Disclaimer: Curated by HT Syndication.